Woodworking

Surface Prep: Planing, Scraping, Sanding

A finish magnifies whatever is under it. Smooth with a sharp plane where you can, scrape the tearout, and sand through the grits without skipping - then check with raking light before the first coat.

  • 4 min
  • 5 steps
  • 3 questions
  • Lesson 42 of 160

In this lesson

  1. Planing
  2. Scraping
  3. Sanding
  4. Inspect before finishing
  5. What to take from this

Planing

The best surface for most finishes comes straight off a sharp, finely set smoothing plane. The blade severs the fibers cleanly, leaving a surface that’s flat, crisp, and clear, without the fine scratches and packed dust of sanding. Pre-industrial furniture was finished from the plane and scraper, and its subtle tool marks are part of its look 1.

A hand holding a thin rectangular steel scraper against the curved spruce top of a violin, with fine shavings around it.
A violinmaker finishing an arched top with a card scraper, a thin steel blade that works almost like an ultrafine plane. Credit: Violinmaker Jacob von der Lippe · CC BY-SA 2.0 · Source

For a finish-ready planed surface:

  • Hone the smoother just before final passes.
  • Set it for the finest shaving that cuts full width.
  • Set the cap iron close and the mouth tight.
  • Plane with the grain, overlapping passes.
  • Ease arrises (sharp edges) with a block plane or a few strokes of fine sandpaper.

Quick check

Why is a planed surface often better than a sanded one under a finish?

Scraping

A card scraper - a thin rectangle of steel - takes gossamer shavings with a tiny hook turned on its edge. It’s the cure for tearout in figured or reversing grain, where every plane direction tears, and for leveling small areas.

Sharpening (see the video):

  1. Joint the edge square with a mill file.
  2. Hone the edge and faces on a stone to remove file marks.
  3. Burnish: draw a hardened burnisher along each face, then along the edge at a slight angle, to turn a small hook.

To use it, hold it with both hands, flex it slightly with your thumbs, tilt it forward, and push (or pull). A sharp scraper makes shavings, not dust. Cabinet scrapers hold the blade in a frame for larger surfaces.

How to sharpen a Thin Scraper | Paul Sellers Sharpening a card scraper - file the edge square, hone it, then turn a burr with a burnisher. Credit: Paul Sellers · YouTube standard license · 7:22 · Source

Playback is optional. If the player is unavailable, open the video at its source.

Quick check

What cuts with a card scraper?

Sanding

Sanding is the most common prep and the least pleasant. Rules:

  • Start with the coarsest grit needed to remove defects and machine marks - often 120 on planed wood, 80 or 100 on rough or machine-planed boards.
  • Don’t skip grits: each one should just remove the scratches of the last. Skipping leaves deeper scratches that the finer grit can’t reach and that show under finish 2.
  • Stop at the right grit for the finish: typically 150 to 180 under a film finish or paint, and 180 to 220 under oil; very fine sanding can keep stain from penetrating evenly 2.
  • Sand with the grain for the final grit; cross-grain scratches stand out.
  • Use a block on flat surfaces; fingers sand hollows.
  • Clean between grits (vacuum or a brush) so loose coarse grit doesn’t scratch at the next stage.
  • Wear a respirator: sanding makes the most hazardous fine dust in the shop (see Dust Collection).

Raise the grain before a water-based finish or dye: wipe with a damp cloth, let dry, and lightly sand off the raised fibers with the final grit.

Quick check

Why shouldn’t you jump from 80-grit straight to 220-grit sandpaper?

Inspect before finishing

Turn off overhead lights and shine a light low across the surface (raking light). Look for:

  • Plane tracks and ridges.
  • Tearout and fuzzy grain.
  • Sanding swirls and cross-grain scratches.
  • Dried glue, which repels stain and finish (a wipe with mineral spirits makes it show).
  • Dents (steam them out with a damp cloth and a hot iron).

Fix them now; finish will only magnify them.

What to take from this

Smooth with a sharp, finely set plane where you can, and scrape tearout with a burnished card scraper. When sanding, start only as coarse as needed, step through every grit, finish with the grain, and stop around 150-180 for film finishes or 180-220 for oil. Raise the grain before water-based finishes, and inspect in raking light for glue, swirls, and tearout before the first coat.

Lesson complete

Nice work.

1day streak
0/1today's goal
–correct

Up next · 4 min

Oil and Wax Finishes

Next lesson
Sources for this lesson
  1. 1
    Joshua A. Klein. The Foundations Course (Apprenticeship Series). Mortise & Tenon Magazine. verifiedHand-tool furniture making from pre-industrial originals - tool selection, sharpening, lumber processing, mortise and tenon, through and half-blind dovetails, nailed rabbets, dados, and shellac and milk paint finishes.
  2. 2
    What Grit Should I Use for Prep Sanding Raw Wood?. General Finishes. verifiedWork up through grits without skipping; 120-150 for paint, up to 180 for open-grain wood under water-based stain, 150-220 for closed-grain woods.